Aluminum bending coefficients regularly, generally aluminum thickness of 0.8 times, such as 3mm, aluminum bending coefficient is 2.4,5mm aluminum bending coefficient is 4.
Use a knife knife is commonly used, it is better to too much stress with a straight sword knife, aluminum easily cracked.
Causes of cracking aluminium plate bends 180 degrees
1, bend the edges with aluminum plate parallel to the rolling direction, which is very easy to crack, bend direction 90 degrees.
2, 180-degree bend angle too much, to be greater than the minimum bend RADIUS, bend RADIUS is 1.5 times times the thickness
3, material reasons, aluminum alloy, good toughness is pure aluminum plate, easy to crack.
4, plate thickness is too thick, bent 180 degrees out of the bending limit.
Related News
- What is Waterstain on Aluminum
- Why Aluminum Alloy For Automobi
- A Brief Introduction for Pure A
- The Difference of Mechanical Wo
- Pattern aluminum-related knowle
- Sectionalized Double Bus Bar
- Aluminum in Transport
- Aluminum Used for Bicycle
- How to Make Aluminum Foil ?
- What Are Aluminum Alloys for Bi
- Properties of Aluminum
- Aluminum and Aluminum Alloy's A
- How to Calculate the Weight of
- Why Anodization for Aluminum ?